Page 3 of 3

Posted: Thu Jun 04, 2009 1:00 pm
by Bob_A
Jo Pea wrote:They recommended 'Resiply'. Any comments?
Seems they have a website
http://www.resiply.co.uk/

I wonder if it's any good?

Posted: Thu Jun 04, 2009 8:07 pm
by jay-Manor Driveways
looks good

Posted: Thu Jun 04, 2009 8:43 pm
by Jo Pea
thanks for pointing out web site. not very technically put together i thought tho. seems fair enough that you can just mix as much as you need BUT has anybody out there used it plse?
jo

Posted: Thu Jun 04, 2009 10:35 pm
by lutonlagerlout
sydneycity wrote:LLL,

Hello mate. Got the Rompox Easy in yesterday evening (took six tins, i ordered seven..phew). Started at 5pm when still very warm and it was going off quick, finished at 9pm. One thing i was a bit worried about was that some of the tins had not mixed/had large hard lumps of greenish (presumably either a hardening agent or resin) compound. I tried to break it up and mix it in with some success. This applied to about half of the tins. Still ,all looks to have gone off okay. I'll forward some pics soon.
if anyone can do ,sydney can
the man is a machine,best non building worker i have worked with
LLL

Posted: Fri Jun 05, 2009 8:24 am
by Rich H
Just had a chat with them. Seems it compares with the Romex D1/D2 products. Need some testimonials.