Hi, we have had a new patio laid but the pointing is already crumbling in places. It’s only been down a couple of weeks. The slabs were laid in the extream heat in full sun. One day was mid 30 degrees. I’m concerned that the Heat has caused it to dry out too quickly. If this is the case what would be the solution?
Thanks
Posted: Tue Aug 14, 2018 11:00 pm
by lutonlagerlout
Rake it out and repoint it on a cooler day
basically the mortar has cooked,dried out before it cured
the installer should have known this
LLL
Posted: Wed Aug 15, 2018 10:32 am
by Paul.p
Thanks, that's what I thought.
Will this also have caused issues with what the slabs were laid on also?
Thanks
Posted: Sat Aug 18, 2018 6:07 pm
by lutonlagerlout
not necessarily
pointing is more susceptible as it is in full sun