Posted: Mon Jun 30, 2014 5:17 pm
Hi Folks
What a great website it inspired me to do a bit of paving, 18 sq/m of Indian sandstone. Flags are layed on concrete with 20-30mm sharpsand/cement bedding. Job was going well until I did the pointing. I used sharpsand/cement 4 to 1 semi-drymix with a touch of plasticiser. Joints vary between 8-14mm. I packed the pointing into the joints.
I did this yesterday which was quite hot day so after pointing I used a water spray bottle to dampen the mix. 24 hours later I find that the pointing hasnt set hard still loose. Can anyone shed any light waht has gone wrong please?
Thanks
What a great website it inspired me to do a bit of paving, 18 sq/m of Indian sandstone. Flags are layed on concrete with 20-30mm sharpsand/cement bedding. Job was going well until I did the pointing. I used sharpsand/cement 4 to 1 semi-drymix with a touch of plasticiser. Joints vary between 8-14mm. I packed the pointing into the joints.
I did this yesterday which was quite hot day so after pointing I used a water spray bottle to dampen the mix. 24 hours later I find that the pointing hasnt set hard still loose. Can anyone shed any light waht has gone wrong please?
Thanks