Page 1 of 1

Posted: Mon Feb 29, 2016 7:13 pm
by diy_jim
Hi,

Im ready to lay my edging kerbs, i plan on using a semi dry mix as mentioned on this site for bedding and a slightly moist one for haunching. The weather has been around 6 or 7 degrees during the day but the last few nights have seen it drop to around 0. Is this going to be ok, or should i should I use an additive?? If so, what do i use??

Thanks

Posted: Mon Feb 29, 2016 7:17 pm
by mickg
lay the kerbs, haunch both side to hold them in position and cover with hessian

Posted: Mon Feb 29, 2016 9:37 pm
by diy_jim
Thanks for the quick reply.