Page 1 of 1

Posted: Thu Aug 29, 2013 11:51 am
by bodgeitandscarper
Somebody has asked me repoint 2 course of bricks and was just wondering what the mix should be and any tips!

Posted: Thu Aug 29, 2013 4:32 pm
by lutonlagerlout
is it hydraulic lime or hydrated?
if they just want it to look creamier than new mortar i would go 5 sand:1lime:1 cement

however traditional lime mortar contains no cement at all

the biggest problem for you is that lime comes in 25kg bags :;):
LLL

Posted: Thu Aug 29, 2013 5:31 pm
by bodgeitandscarper
It's the two bricks below damp course, it's been painted previously but the paint has come off and the pointing has gone. Once it's been reprointed , he will repaint.

Posted: Thu Aug 29, 2013 7:38 pm
by digerjones
i would'nt bother with lime if its going to be painted. i would use 3 to 1 cement mortar.

Posted: Thu Aug 29, 2013 8:53 pm
by lutonlagerlout
yeah especially below dpc
LLL

Posted: Thu Aug 29, 2013 9:46 pm
by bodgeitandscarper
Thanks for the replies.

I did suggest this but apparently because its a really old building, it needs it, as cement mortar would be problematic, something to do with moisture.

Posted: Thu Aug 29, 2013 9:51 pm
by bodgeitandscarper
I emailed him earlier and he says although from outside it looks like it has a dpc (render stops @ floor level) it doesn't so that's why it requires lime mortar?

Maybe I shouldn't do this favour!