I've got some marshalls eclipse granite to joint and following marshalls laying instructions the joints are only 5mm wide, I spoke to easipoint about there gun point but they said although it says 5mm upwards you will struggle to get it in properly, so they recommended sett point slurry. I've also spoke to ncc streetscape about their slurry, has anybody had any experience with these and is it easy to clean the surface after? Any other suggestions welcome and I need it to be black or dark grey, thanks. :)
Paving and Groundworks in Lincolnshire

01526 342202 07774 424275

Pablo
Posts: 1990
Joined: Sun Mar 25, 2007 10:49 pm
Location: N/Ireland

Post: # 64244Post Pablo

If you're slurrying smooth granite with narrow joints then you may as well use 3:1 sand & cement it'll be seriously cheaper and look just as good. A squeegee and soft brush is all you need and a bit of patience. I've slurried a fair bit of Eclipse and it's always looked very well.
Can't see it from my house

ilovesettsonmondays
Posts: 1071
Joined: Sat Aug 22, 2009 8:57 pm
Location: essex

Post: # 64245Post ilovesettsonmondays

belt cleaner is what we use on setts whenslurry pointing and sponge on bits the belt cleaner cant get . get as much slurry off as possible with squeegy and keep setts misted with water

msh paving
Site Admin
Posts: 1854
Joined: Tue Aug 19, 2008 7:03 pm
Location: kings lynn norfolk
Contact:

Post: # 64247Post msh paving

speak to cookie, hes the man for that job MSH :D
paving, mini-crusher, mini-digger hire and groundwork
http://mshpaving.co.uk

pickwell paving
Posts: 190
Joined: Wed Jul 14, 2010 8:27 pm
Location: lincs

Post: # 64258Post pickwell paving

Thanks lads, i've only got 60 sqm to do and with the joints been quite narrow the cost isn't that bad especially for the sett point stuff, easipoint recommended using a mop with a sponge on the end to clean them after, just didn't want to risk staining them as there's quite a bit of money's worth of slabs.
Paving and Groundworks in Lincolnshire

01526 342202 07774 424275

mickavalon
Posts: 661
Joined: Mon Feb 21, 2005 11:54 am
Location: Birmingham, west midlands, UK
Contact:

Post: # 64312Post mickavalon

Just keep a fine mist on it mate, as long as you dont go and do too big an area until you've sussed it out, you'll be fine. We sometimes mix 1.5 building sand, 1.5 Silver sand, half rapid set and half normal cement, pour it in and wipe back off with floor tilers grouting sponges and bucket. Works a treat. Just do a small section first.