Possible acid damage to real slate flagstones - Spoilt patio/pathway slate
-
- Site Admin
- Posts: 4420
- Joined: Sat Aug 09, 2008 3:55 pm
- Location: high peak
- Contact:
wide joints and 4 corners touching in a few places, yeah they are level but thats about it,
Giles
Groundworks and Equestrian specialists, prestige new builds and sports pitches. High Peak, Cheshire, South Yorkshire area.
http://www.gbgroundworks.com
Groundworks and Equestrian specialists, prestige new builds and sports pitches. High Peak, Cheshire, South Yorkshire area.
http://www.gbgroundworks.com
-
- Posts: 9
- Joined: Thu Oct 07, 2010 7:30 pm
- Location: Pembrokeshire
Thanks to London Stone Paving for posting my photos.
Rightly or wrongly, we managed to clean the slate up with stainless steel wool (advised by a local builder who has done a lot of work with slate). They've come up really good, (no efflorescence) only problem they are very pale in colour. Just as they were when the builders used the acid. Remnants of that possibly (does acid lighten slate ?) Builders want to use ltp colour intensifier and stain block but we are so scared it'll cause the whiteness/efflorescent to re-appear. In anycase, we don't know how long the product will last. Don't want to have to re-apply every year or so, and also would the rain droplets stain it. (done a test with a similar paving sealer and the rain drops stained it all). Any ideas whether we should do this or not ? Thanks in advance for any replies. So good to have this forum. Lot of helpful information here.
Rightly or wrongly, we managed to clean the slate up with stainless steel wool (advised by a local builder who has done a lot of work with slate). They've come up really good, (no efflorescence) only problem they are very pale in colour. Just as they were when the builders used the acid. Remnants of that possibly (does acid lighten slate ?) Builders want to use ltp colour intensifier and stain block but we are so scared it'll cause the whiteness/efflorescent to re-appear. In anycase, we don't know how long the product will last. Don't want to have to re-apply every year or so, and also would the rain droplets stain it. (done a test with a similar paving sealer and the rain drops stained it all). Any ideas whether we should do this or not ? Thanks in advance for any replies. So good to have this forum. Lot of helpful information here.
-
- Posts: 1270
- Joined: Mon Aug 10, 2009 8:30 am
- Location: york work anywhere where the stone takes me
- Contact:
-
- Posts: 2199
- Joined: Mon May 10, 2010 1:07 pm
- Location: Surrey
- Contact:
Looks better now. I like the pattern, not seen that one before.
You say the builders want to use LTP on it. I wouldn't let them anywhere near it. Dont rush in to seal it. Speak to extensive and take some sound professional advice.
http://i814.photobucket.com/albums/zz65/StevenWalley/IMG_1111.jpg
http://i814.photobucket.com/albums/zz65/StevenWalley/IMG_1109.jpg
http://i814.photobucket.com/albums/zz65/StevenWalley/IMG_1107.jpg
You say the builders want to use LTP on it. I wouldn't let them anywhere near it. Dont rush in to seal it. Speak to extensive and take some sound professional advice.
http://i814.photobucket.com/albums/zz65/StevenWalley/IMG_1111.jpg
http://i814.photobucket.com/albums/zz65/StevenWalley/IMG_1109.jpg
http://i814.photobucket.com/albums/zz65/StevenWalley/IMG_1107.jpg
-
- Posts: 9
- Joined: Thu Oct 07, 2010 7:30 pm
- Location: Pembrokeshire
Hi everyone
Thanks London Stone Paving for uploading my photos. Much appreciated.
We've phoned LTP and they say the slates have turned pale because of all the chemical treatment. They say colour intensifier would help. To cut a long story short. As we've now got them back into a reasonable condition (something we can now live with) we've decided not to put any further chemicals on them, or indeed to do anything else other than the occasional wash. LTP told us if we applied their colour intensifier it would have to be redone every 3yrs or so plus continual maintenance of a wash/wash. I suppose it's all a learning curve for all of us. Just hope all this intensive chemical treatment hasn't caused any detrimental damage to the slates. Does anyone know whether it has ?
Thanks everyone for your help. Hope our unfortunate incident will help others wanting to instal a slate patio/pathway.
Thanks London Stone Paving for uploading my photos. Much appreciated.
We've phoned LTP and they say the slates have turned pale because of all the chemical treatment. They say colour intensifier would help. To cut a long story short. As we've now got them back into a reasonable condition (something we can now live with) we've decided not to put any further chemicals on them, or indeed to do anything else other than the occasional wash. LTP told us if we applied their colour intensifier it would have to be redone every 3yrs or so plus continual maintenance of a wash/wash. I suppose it's all a learning curve for all of us. Just hope all this intensive chemical treatment hasn't caused any detrimental damage to the slates. Does anyone know whether it has ?
Thanks everyone for your help. Hope our unfortunate incident will help others wanting to instal a slate patio/pathway.
-
- Posts: 9
- Joined: Thu Oct 07, 2010 7:30 pm
- Location: Pembrokeshire
-
- Site Admin
- Posts: 15184
- Joined: Fri Aug 04, 2006 12:20 am
- Location: bedfordshire
-
- Site Admin
- Posts: 4420
- Joined: Sat Aug 09, 2008 3:55 pm
- Location: high peak
- Contact:
Wonder why they didn't lay them more random than then regular straight joint every 600mm they've got? Like brick bond etc?
Giles
Groundworks and Equestrian specialists, prestige new builds and sports pitches. High Peak, Cheshire, South Yorkshire area.
http://www.gbgroundworks.com
Groundworks and Equestrian specialists, prestige new builds and sports pitches. High Peak, Cheshire, South Yorkshire area.
http://www.gbgroundworks.com
-
- Site Admin
- Posts: 15184
- Joined: Fri Aug 04, 2006 12:20 am
- Location: bedfordshire
-
- Posts: 9
- Joined: Thu Oct 07, 2010 7:30 pm
- Location: Pembrokeshire
Had to do the design ourselves as the builder didn't have a clue. Whilst he laid the slate fairly well, he knew very little about anything else. He even got the pattern wrong on one section! We were told not to buy slate too heavy i.e. too big slabs, hence only two sizes.
The Company in question deal mainly with tarmacadam/council paths/road works and have branched out into patio laying. Unfortunately we were'nt aware of this and I suppose were used as guinea pigs. We're rather disappointed that our slates had such bad treatment with all the chemicals leaving them a light lighter but with hindsight if they hadn't grounted in the rain this would never have happened. It's all too late now to do anything about it.
We thought we had employed a Company with expertise/patio laying skills. Obviously not. The tarmacadam was perfect.
The Company in question deal mainly with tarmacadam/council paths/road works and have branched out into patio laying. Unfortunately we were'nt aware of this and I suppose were used as guinea pigs. We're rather disappointed that our slates had such bad treatment with all the chemicals leaving them a light lighter but with hindsight if they hadn't grounted in the rain this would never have happened. It's all too late now to do anything about it.
We thought we had employed a Company with expertise/patio laying skills. Obviously not. The tarmacadam was perfect.