Post: # 45284Post dr benway

thanks all, for the replies

the slabs arent rocking, so as Tony suggests, I'll wait and see.

thanks

lutonlagerlout
Site Admin
Posts: 15184
Joined: Fri Aug 04, 2006 12:20 am
Location: bedfordshire

Post: # 45288Post lutonlagerlout

cookiewales wrote:
lutonlagerlout wrote:i thought unibond was PVA?
definitely wouldn't use any additives in the pointing,even the dyes leach out fast
LLL

unibond is a sbr in most cases take a look on the tin :p ??? ???
in that case I am ok as i have always used unibond :)
LLL
"what,you want paying today??"

YOUR TEXT GOES HERE

lutonlagerlout
Site Admin
Posts: 15184
Joined: Fri Aug 04, 2006 12:20 am
Location: bedfordshire

Post: # 45289Post lutonlagerlout

bah just checked and they make PVA too
IME I have never had a problem with unibond PVA in the mix
maybe i have been lucky :)
LLL
"what,you want paying today??"

YOUR TEXT GOES HERE

Tony McC
Site Admin
Posts: 8346
Joined: Mon Jul 05, 2004 7:27 pm
Location: Warrington, People's Republic of South Lancashire
Contact:

Post: # 45338Post Tony McC

Plastering sand is a little bit sharper than building sand but nowhere near as coarse as sharp/grit/concreting sand. It is normally used to create a scratch coat.

You have to be careful with it when laying the Indian sandstone as it can contain a lot of iron that gets carried through the stone causing discolouration.

Nice of you to ask about the Boddies, Craig: didn't you owe me a pint or three? :D
Site Agent - Pavingexpert

Craig2
Posts: 31
Joined: Thu Jul 24, 2003 10:39 pm
Contact:

Post: # 45362Post Craig2

:D I guess I am not alone in owing you a pint or two...

I have had some discolouration issues but only with the Grey/blue and not consistantly but with the occasional job, gotta admit It had me stumped.

Back on topic, I just thought I should mention the success I've had with the SBR OPC 50/50 slurry bond.
I trialed 5 indianstone 100mm cobbles with varying different bonding techniques, 24 hours later I tried them all with reasonable force and only one lifted, which was the most liberally treated, it was still wet and I replaced it,I tried them again today and I swear I could have swung from them, they were not for moving,believe me when I say I tried.
I have refit the lot now, mixing in a billy can with 1 cup of SBR and 1 cup of Cement and stirring until I got a constant colour/consistancy, I then dipped the lower part of the cobble in the can and let the excess drip off for a moment and then down,I applied a little pressure until you can see the mixture being squeezed from underneath, you get a certain amount of adhesion straight away, I was suitably Impressed!!

I agree with Tony though, if they are not moving then there is little problem, however I can't see me being able to convince a customer so...lol

simeonronacrete
Posts: 373
Joined: Tue Feb 18, 2003 3:11 pm
Location: Essex
Contact:

Post: # 45579Post simeonronacrete

Generally a mortar or concrete made with sharp sand is stronger than using soft sand. Also more likely to achieve water resistance as there are fewer gaps in the matrix.

Unibond is PVA, not SBR. PVA's break down in contact with water, liquid or vapour, SBR doesn't.

Ronafix is based on SBR and IS waterproof, IS watertight, and WILL bond securely to building surfaces.
Simeon Osen
Ronacrete Ltd - http://www.ronacrete.co.uk
Tel: +44 (0) 1279 638 700
Follow us at http://www.twitter.com/Ronacrete

Tony McC
Site Admin
Posts: 8346
Joined: Mon Jul 05, 2004 7:27 pm
Location: Warrington, People's Republic of South Lancashire
Contact:

Post: # 45593Post Tony McC

What Sim is trying to say in his polite way is that Ronafix/SBR sticks like the proverbial to a blanket! :D
Site Agent - Pavingexpert

lutonlagerlout
Site Admin
Posts: 15184
Joined: Fri Aug 04, 2006 12:20 am
Location: bedfordshire

Post: # 45595Post lutonlagerlout

i went in 3 BMs today and none of them had SBR
when i asked why,they said they can get it but its so expensive no one stocks it
LLL
"what,you want paying today??"

YOUR TEXT GOES HERE

GB_Groundworks
Site Admin
Posts: 4420
Joined: Sat Aug 09, 2008 3:55 pm
Location: high peak
Contact:

Post: # 45598Post GB_Groundworks

last time i bought it last year was about £15/5 litres sealocrete branded one from local independent bm
Giles

Groundworks and Equestrian specialists, prestige new builds and sports pitches. High Peak, Cheshire, South Yorkshire area.

http://www.gbgroundworks.com

Bob_A
Posts: 861
Joined: Wed Feb 27, 2008 9:30 pm
Location: SE London/ NW Kent

Post: # 45609Post Bob_A

At Toolstation 5L of SBR is £16.37 and 5L of pva is £7.48.
After reading about SBR on here it seems worth the extra money and in most cases in the future I'll be using it in preference to pva.

Tony McC
Site Admin
Posts: 8346
Joined: Mon Jul 05, 2004 7:27 pm
Location: Warrington, People's Republic of South Lancashire
Contact:

Post: # 45612Post Tony McC

BMs - the curse of the building trade (along with architects).

How many time have we been told that they don't stock such-and-such because there's no demand. Eh?? I'm here, now, demanding it!

Never forget that BMs are run for *their* benefit, not the benefit of contractors or manufacturers/suppliers, and they will only ever stock items that they can shift in volume and at a hefty profit, after screwing the manufacturer on pricing and then screwing the contractor on cost.
Site Agent - Pavingexpert

lutonlagerlout
Site Admin
Posts: 15184
Joined: Fri Aug 04, 2006 12:20 am
Location: bedfordshire

Post: # 45616Post lutonlagerlout

i have told butterfields and dandys that geo-fix is rubbish,yet they both still stock it sky high for the unsuspecting mugs
they have targets to meet
LLL
"what,you want paying today??"

YOUR TEXT GOES HERE

ambient
Posts: 393
Joined: Fri Jun 13, 2008 6:20 pm
Location: bolton lancs
Contact:

Post: # 45675Post ambient

been in travis perkins today they stock two brands of sbr ???
ambientdriveways.co.uk ambientexcavations-bolton.co.uk

cookiewales
Posts: 1270
Joined: Mon Aug 10, 2009 8:30 am
Location: york work anywhere where the stone takes me
Contact:

Post: # 45682Post cookiewales

Unibond is PVA, not SBR. PVA's break down in contact with water, liquid or vapour, SBR doesn't. i have been useing ronofix since 1987 never failed me yet best to buy in 25 litre drums it dosent go off am sure when my eyes could read the back of a tin it said sbr as well on the unibond i was looking at was a long time ago ??? :;):
Originalstonepaving.com

The very best in natural stone paving in new and reclaimed materials
M: 07968 582231

lutonlagerlout
Site Admin
Posts: 15184
Joined: Fri Aug 04, 2006 12:20 am
Location: bedfordshire

Post: # 45686Post lutonlagerlout

well after 26 years at work, used SBR on some rendering today
met the labourer tonight in "the compasses" and both of us have it stuck all over our hands
will report update tomorrow