Dry or wet bedding mix? - Indian sandsone flags
-
- Posts: 37
- Joined: Fri Apr 05, 2002 10:56 pm
- Location: Malvern
In the past I have used a dry mix to do some utility areas and as I used a fairly strong mix they have been fine. I have 50 sqm of Indian sandstone to lay and have started by doing the steps and for this I used a wet mix and that is also fine.
I'm now trying to decide which is the best bedding to use for the rest of the patio. Can someone tell me the pros and cons please?
I'm now trying to decide which is the best bedding to use for the rest of the patio. Can someone tell me the pros and cons please?
Andyfr
-
- Posts: 884
- Joined: Thu Feb 08, 2007 12:28 pm
- Location: Reading
IMO the stronger the mix the more water you need. This is because the cement uses the water as it reacts. If you don't have enough, the mix can dry out before curing enough to bond to the slab. I like to use a ratio of about 4:1 with the slump set to just about bind but also break up easily. Indian sandstone is pretty 'thirsty' so better to be slightly too wet than too dry.
-
- Posts: 17
- Joined: Fri Dec 28, 2007 4:45 pm
- Location: Yorkshire
-
- Posts: 24
- Joined: Tue Jun 20, 2006 7:46 am
- Location: Shavington, Cheshire
- Contact:
My 2p worth.. I use a measured (14L bucket), plasticised 3:1 mix. Wet. Trowel in around the edge of the last piece you laid then in to the bed. Fill where the joint will be before you lay the stone. Gently push the stone in to place (a few taps with a rubber mallet if you can't push with your hand) and you have a 3:1 joint completely consolidated on a full bed - no pointing needed and it won't come out. You never get a rocker. They are easy to place and once you take off the excess pushed up in the joint and strike off the top of the joint it's done. Move on to the next piece.
-
- Site Admin
- Posts: 15184
- Joined: Fri Aug 04, 2006 12:20 am
- Location: bedfordshire
-
- Posts: 1990
- Joined: Sun Mar 25, 2007 10:49 pm
- Location: N/Ireland
-
- Posts: 24
- Joined: Tue Jun 20, 2006 7:46 am
- Location: Shavington, Cheshire
- Contact:
Fairy will plasticise but will also weaken the mix. The green dye in Fairy can also change the colour of the mortar.
"Feb" or "Addmix" is just as cheap and won't make air bubbles that Fairy can.
A 25L drum of Feb from B&Q is about £15. That'll last for over 200 bags of cement if you add a 125ml per mix to each bag of cement.
"Feb" or "Addmix" is just as cheap and won't make air bubbles that Fairy can.
A 25L drum of Feb from B&Q is about £15. That'll last for over 200 bags of cement if you add a 125ml per mix to each bag of cement.
-
- Site Admin
- Posts: 15184
- Joined: Fri Aug 04, 2006 12:20 am
- Location: bedfordshire
-
- Posts: 368
- Joined: Tue Sep 25, 2007 7:20 pm
- Location: darwen
- Contact: