Help! need advice on moisture stains on paving.

Patio flagstones (slabs), concrete flags, stone flags including yorkstone and imported flagstones.
Post Reply
AAA10
Posts: 4
Joined: Tue Jul 19, 2016 3:44 pm
Location: Northampton

Post: # 110223Post AAA10

Hi, I recently (couple weeks ago) had some sawn sandstone paving installed, and have been having problems with what appears to be trained moisture stains. The paving was laid on a full bed of mortar (not spot bedded) so I'm struggling to understand what is causing it. Any pearls of wisdom are most welcome!

Thanks


http://s1052.photobucket.com/compone....e_3.jpg

http://s1052.photobucket.com/compone....e_3.jpg
AAA

lutonlagerlout
Site Admin
Posts: 15184
Joined: Fri Aug 04, 2006 12:20 am
Location: bedfordshire

Post: # 110227Post lutonlagerlout

that looks tidy,but the joints are a little tight for my liking
why has it not been pointed?
some sort of moisture issue there but theoretically it should dry out ,sooner rather than later
looks a good job
LLL :)
"what,you want paying today??"

YOUR TEXT GOES HERE

AAA10
Posts: 4
Joined: Tue Jul 19, 2016 3:44 pm
Location: Northampton

Post: # 110231Post AAA10

Thanks for the reply bud. I'm hoping your right, as with this heat wave I thought they would be dry by now! Should I avoid sealing until they clear up??
AAA

seanandruby
Site Admin
Posts: 4713
Joined: Mon Jun 26, 2006 11:01 am
Location: eastbourne

Post: # 110232Post seanandruby

Yes let them dry completly.
sean

Tony McC
Site Admin
Posts: 8346
Joined: Mon Jul 05, 2004 7:27 pm
Location: Warrington, People's Republic of South Lancashire
Contact:

Post: # 110240Post Tony McC

There are two most likely causes. It could be either or it could be a bit of both.

First, it could be that the damp flags are slightly more porous than the dry flags and so are wicking/retaining moisture more readily.

Secondly, it could be that the bedding mix is different beneath the damp and the dry flags.

What strikes me is that it seems to be affecting whole flags (more or less) which suggests it's not something systemic but a variable which impacts on certain flags only. I know there is one flag that looks damp-ish but that could be a transition piece, halfway between the damp and the dry.

And those joints need sealing with summat otherwise they are just going to collect crap.
Site Agent - Pavingexpert

AAA10
Posts: 4
Joined: Tue Jul 19, 2016 3:44 pm
Location: Northampton

Post: # 110243Post AAA10

Tony McC wrote:There are two most likely causes. It could be either or it could be a bit of both.

First, it could be that the damp flags are slightly more porous than the dry flags and so are wicking/retaining moisture more readily.

Secondly, it could be that the bedding mix is different beneath the damp and the dry flags.

What strikes me is that it seems to be affecting whole flags (more or less) which suggests it's not something systemic but a variable which impacts on certain flags only. I know there is one flag that looks damp-ish but that could be a transition piece, halfway between the damp and the dry.

And those joints need sealing with summat otherwise they are just going to collect crap.

Thanks for the replies!

Yes I will get the joint filled, it had kiln dried sand in there, but it blew out when I pressure washed the slabs.

I'm fairly certain the guy used the same bedding mix all the way round. It's just bizarre how the pattern of patchiness is spread. It's not typical picture framing or spot bedding.

From what you guys are saying, it doesn't sound like it should be terminal, so I'm going to be patient and see if it dissipates over the next few weeks!
AAA

Tony McC
Site Admin
Posts: 8346
Joined: Mon Jul 05, 2004 7:27 pm
Location: Warrington, People's Republic of South Lancashire
Contact:

Post: # 110265Post Tony McC

If you are going to be pressure washing this pavement regularly, then look to use a joint stabiliser with the KDS so that you don't lose the sand every time you clean.
Site Agent - Pavingexpert

AAA10
Posts: 4
Joined: Tue Jul 19, 2016 3:44 pm
Location: Northampton

Post: # 110272Post AAA10

Tony McC wrote:If you are going to be pressure washing this pavement regularly, then look to use a joint stabiliser with the KDS so that you don't lose the sand every time you clean.
Yes that's a good shout!
AAA

Post Reply