Quick question, how do you do a flushed joint with a trowel without getting mortar over the slabs?! Surely it's just pulling the trowel along the height of the slab edges so that it sits flat in it but can't see from having not done it before how you avoid it draggin onto the slabs??
I'm just a useless bellend
-
- Posts: 4
- Joined: Thu May 19, 2016 9:26 am
- Location: Colne
-
- Site Admin
- Posts: 15184
- Joined: Fri Aug 04, 2006 12:20 am
- Location: bedfordshire
-
- Posts: 1951
- Joined: Sat Dec 06, 2008 10:28 pm
- Location: Preston, Lancashire
-
- Site Admin
- Posts: 8346
- Joined: Mon Jul 05, 2004 7:27 pm
- Location: Warrington, People's Republic of South Lancashire
- Contact:
There is no good reason to use a vee iron rather than a half-round when it comes to pavement pointing, but they do have their uses on vertical masonry.J McNulty wrote:What's the purpose of a "vee pointer" compared to a normal one?
On a horizontal surface vee-joints allow water to hang around too long and they create a joint that rapidly fills with detritus. Half round is a better option, and the shallower the better. Flat (aka weatherstruck) is the best option as there's nowhere for surface water to pool and nowhere for crap to accumulate.
Using the blade of a trowel to create a struck joint inevitably results in a surface that is ever so slightly angled. This is not necessarily a bad thing, but if you have a fancy for a truly flat joint surface, there are flat irons available. For occasional pointers and DIYers not wanting to spend money on a tool they'll only use the once, put a 45° kink in a short length of copper pipe and flatten one end with a hammer.
Site Agent - Pavingexpert
-
- Posts: 24
- Joined: Wed Apr 08, 2015 9:05 am
- Location: Farnborough
Back of a spoon sounds like a good option for different sized joints then!! The flattened copper sounds like a good method though.
So what is the ideal sort of few days for jointing with mortar then? Absolutely bone dry? And how long does it take to go off, ie, how many rain free days do you realistically need to avoid horrors?
So what is the ideal sort of few days for jointing with mortar then? Absolutely bone dry? And how long does it take to go off, ie, how many rain free days do you realistically need to avoid horrors?
I'm just a useless bellend
-
- Site Admin
- Posts: 8346
- Joined: Mon Jul 05, 2004 7:27 pm
- Location: Warrington, People's Republic of South Lancashire
- Contact:
-
- Posts: 24
- Joined: Wed Apr 08, 2015 9:05 am
- Location: Farnborough
yup, seen a few new patios in other people's gardens lately which look like they were jointed during the tiny, tiny hot spell we had and the flags have tiny, tiny cracks alongsidethe mortar. Hey ho.
Annoyingly, today would be perfect if it wasn't for the suspected showers between 8-11 tonight! :rock:
Thanks for the timing/condition advice though.
Annoyingly, today would be perfect if it wasn't for the suspected showers between 8-11 tonight! :rock:
Thanks for the timing/condition advice though.
I'm just a useless bellend